Apply : screen printing Adhesives; Metal sheet and film lamination; Adhesives; Adhesives for different substrates
Features : Ink bonding material; excellent adhesion; FDA certification CFR175.105, 175.300 and 176.170
Performance
parameter |
unit |
Value |
Appearance |
|
yellow Flake solid |
Molecular Weight |
g/mole |
26,000 |
Viscosity |
d.l/g |
0.69 |
Glass transition temperature |
degree C |
17 |
softening point |
degree C |
105 |
acid value |
KOH mg/g |
less than 3 |
OHvalue |
KOH mg/g |
2~5 |
stretch length |
kg /cm2 |
55 |
dissolve Method
Put all the solvents in the reactor, while stirring, put the PT-17 solid into Reactor; after adding all components, raise the reaction temperature to 90-100 degrees, if using MEK and acetone, the reactor temperature rises to 50-60 degrees, stir for two hours, the maximum pressure of the reactor: 2kg/cm 2, turn off the heating system, continue to stir for an hour and a half, let the reactor cool down naturally, stop stirring; filter the solution, put it into a 200kg barrel
applies Solvent : EK, Toluene, xylene, solvesso, cyclohexanone, acid gas cellulose ester, isophorone, DBE
from Original formula : Prevent Back Stick Screen Printing Adhesive
white |
PT-17 16.5parts |
PET or PVC film composite, steel or PET film Formula: PT-17+PT-65
sticky Mixture formula : PT-17+PT-65+Isocyante[L75]
for soft Adhesives for flat cables
PT-17S(50%) 30.0part
PT-65S(50%) 20.0part
TIO2 18.0part
Flame Retardant (Br) 30.0part
Additive 2.0 part
metal Foil Adhesive Recipe : PT-17+ solvent (16~20%)+L75 (5% of solid content)
Packaging :25KG/box
sticky Mixture formula : PT-17+PT-65+Isocyante[L75]
for soft Adhesives for flat cables
PT-17S(50%) 30.0part
PT-65S(50%) 20.0part
TIO2 18.0part
Flame Retardant (Br) 30.0part
Additive 2.0 part
metal Foil Adhesive Recipe : PT-17+ solvent (16~20%)+L75 (5% of solid content)
Packaging :25KG/box